Before accepting a peel strength number, ask the supplier to mark the intended bond on a cross-section and show the two surfaces left after the test. If a backsheet split internally while the backsheet-to-encapsulant bond stayed intact, the force describes a different failure from the one you ordered. Record what the test demonstrated, then decide whether a different specimen or a documented engineering disposition is needed.
A solar module buyer can use a peel report at three different points: selecting a material combination, approving a change to that combination, or accepting evidence about a specific production lot. Each decision needs a different connection between the specimen tested and the product ordered. Start the RFQ by naming the decision. A report for comparing two candidate films can be perfectly useful during design selection even if neither specimen can be traced to the delivery waiting at your warehouse.
Mark the two surfaces on the drawing
An interface is the boundary between two materials in contact. On a glass-backsheet module, the bond between the front glass and the encapsulant is a different interface from the bond between the rear encapsulant and the polymer sheet at the back. A multilayer backsheet can also have several interfaces inside the sheet itself. A drawing with an arrow at the back of the module is ambiguous until the arrow names both materials touching at its tip.
Have the module maker identify the inside face of the backsheet, the grade and revision of the rear encapsulant, and any coating or treatment actually present on the bonded face. Where a controlled code represents a proprietary material, ask for the code and a revision mapping that the supplier can maintain under confidentiality. Purchasing needs enough identity to detect a substitution, while the supplier can keep the formulation private.
Suppose the RFQ is prompted by a change from an opaque rear sheet to a transparent one. Both constructions might have the same power class and external size. Draw the old and proposed rear interfaces side by side, then mark the interface for which the supplier provided a test. An old front-glass report belongs in the historical file. To support the proposed rear combination, the reviewer needs a connection to the new backsheet face, even if the front of the module stays identical. The module glass and backsheet change-control guide covers how to keep those revisions linked to the order.
A buyer sourcing glass-glass modules should request the actual rear-glass surface and film identification. A backsheet interlayer test assumes a polymer sheet containing those layers. Check whether that part even exists in the quoted construction. The IEC technical specification on polymeric front- and backsheets describes characterization of sheet materials and their components, including their combinations with matched materials. Its scope helps identify the appropriate component evidence. The complete module has further qualification requirements that a single interlayer result cannot settle.
Find the fracture plane before comparing the force
Ask the laboratory to name both the bond it set out to test and the path that the separation actually followed. A fracture at the boundary between two materials is called adhesive failure. A fracture inside a material is called cohesive failure. If the backsheet pulled apart between two of its own layers, record those layers. If the peel arm broke while the target bond still held, record the break and where the test stopped.
On small screens, swipe or scroll sideways to read every column. Keyboard users can focus the table and use the arrow keys.
| What the two faces show | How to enter the result |
|---|---|
| Separation stays at the specified boundary | Enter the force statistic and evaluated interval against that interface. |
| Material from the same layer remains on both halves | Describe the cohesive split and ask whether the agreed criterion covers it. |
| An inner backsheet layer leaves with the peel arm | Identify the layers in the backsheet. Keep the requested rear bond open. |
| Grip slip or arm break stops the pull | Record the interruption and available trace. Ask who can authorize a repeat. |
Request pictures of both exposed faces with matching specimen identifiers and an indication of peel direction. A single photograph of the more photogenic side can hide the piece of material that went with the opposite half. A scale or consistent field of view makes it easier to match a local change to a region of the test trace. Ask whoever classified the fracture to label uncertain regions and explain the basis for the classification. Similar-looking thin layers can be hard to identify from a low-resolution image alone.
If the initial segment separates at the target and later diverts into a backsheet layer, the two segments answer different questions. Ask for the part of the trace that belongs to each observed path and how the report treated the transition. A mean across both segments may be repeatable, yet it cannot tell a reviewer the strength of either individual interface without further evidence. Preserve the original trace when requesting a new interpretation, so that the file shows exactly what changed.
There is actual experimental precedent for checking this detail. A Montanuniversität Leoben study on PV encapsulant peel tests examined several encapsulants and backsheets. For one of the materials, aging changed where cohesive fracture occurred. Treat that as a reason to record fracture location at each exposure state. It does not establish which path a different production stack will take.
Read the method and units together
For a conventional peel report, ask whether the reported value is the force divided by specimen width and what portion of the pull contributed to it. A force in newtons alone does not identify the load per unit width. A first peak may represent initiation, and an average over a stated interval may describe continuing separation. Ask the lab which statistic the purchase specification intended before copying a number into the acceptance table.
Here is a dimensional check using a real manufacturer example. Saatvik lists at least 65 N/cm under ASTM D903 for glass peel and gives a separate backsheet peel row for its SS-EPE UVT-F and SS-EPE UVC-B grades. The equivalent unit expression for 65 N/cm is 6.5 N/mm. That conversion only changes the width unit. It does not tell you the identity of a particular delivery, the behavior of a specific backsheet, or the retention of adhesion after a project's conditioning sequence. Saatvik EPE film technical specification
A useful counterexample is 3M's April 2013 technical sheet for EVA9100. Its table lists a typical glass adhesion of 100 N/cm under ASTM D903 and identifies the table as typical data unsuitable for defining specifications. One sheet gives a stated minimum for named products, while the other gives a typical value for another product. Ranking the modules by 100 versus 65 would mix the meaning of the numbers before considering the construction, test conditions or age of the document. The historical sheet is an example of how to read a heading, with current availability and specifications left to the supplier. 3M EVA9100 technical data
A second method may appear alongside peel strength. The single cantilevered beam method uses the behavior of a loaded beam to characterize the energy associated with an advancing separation. IEC TS 62788-6-3 describes this approach for PV laminate interfaces and the comparison of specimens and stress states. Keep beam results reported in energy per area in a separate column from conventional peel-force results. Even where units can be rearranged algebraically, a unit conversion does not account for peel geometry or the work spent deforming a flexible arm. Ask for an agreed common method if the bid decision requires a ranking.
A width correction can sometimes reverse a preliminary bid comparison. Suppose two hypothetical reports use the same geometry and both give a mean force over a stated stable interval. The first gives 30 N on a 10 mm strip and the second 48 N on a 20 mm strip. Entering force per width gives 3.0 N/mm and 2.4 N/mm respectively. The larger force came from the wider specimen. Before ranking either offer, still check the failure faces, material and exposure state. If the wider strip tore inside its backsheet while the narrower one separated at the specified interface, retain the calculation but leave the interface comparison open. These example forces are arithmetic inputs, not product data or acceptance thresholds.
Check what the specimen represents
Have the supplier classify the specimen as a film or sheet maker's reference sample, a separately laminated witness coupon, a piece prepared from an identified module, or another explicitly described construction. Each class can be useful. A film maker's sample can narrow the choice of films. A witness coupon can help monitor an agreed production process without sacrificing a saleable panel. A specimen taken from a known panel answers a question about that panel and location. Keep those descriptions visible in the report heading.
For a witness coupon, trace the materials and process in two directions. First identify which production materials, bonded faces and lamination record the coupon shares with the quoted module. Then list any differences that were necessary to make the specimen peelable. A coupon may omit cells, contain a prepared starter tab, or have a stiff backing attached for the test. Ask which differences the test engineer considers relevant to the target interface. The explanation can be short, but it should address the construction you are buying.
Location matters when someone proposes that strips from one panel demonstrate lot uniformity. Six adjacent strips from one corner provide six observations of that local region. They provide no direct observations of other panel positions or production runs. Ask for separate counts of strips, coupons, panels, material lots and days or shifts represented. Give the sampling plan to the engineering owner before shipment. Let the owner decide how much evidence is proportionate to the commercial exposure and the purpose of the test.
If destructive sampling from a completed module is proposed, confirm who supplies it, who owns it after the examination, and what happens to its serial number in the delivery list. Purchasing should avoid quietly counting that module both as a laboratory specimen and as a unit available for installation. An approved witness coupon may answer a process-control question at lower cost. It still takes a written rationale to use that coupon to settle an issue seen on a returned module.
Compare like specimens before and after conditioning
Request the preparation date, exposure sequence, post-exposure handling, time between conditioning and test, test environment and specimen orientation. Where the supplier describes a sample as fresh, clarify whether that means an unlaminated sheet, an initially laminated coupon, or a sample that has already seen a thermal exposure. Group specimens by actual state before calculating changes. A shelf sample from a material library and a coupon from a newly approved run do not become a matched pair because their labels contain the same film brand.
Peeling consumes the tested path. Ask how the laboratory paired initial and conditioned specimens, especially when the report describes a percentage retained. In many purchasing comparisons the appropriate pair consists of sister specimens cut from a documented construction. Record the lots and positions represented, the statistic used for each group, and whether fracture location remained comparable. A percent without the initial and final values, units and population can conceal either a low starting value or a change in the failure mechanism.
Request the geometry, the angle at which the free arm was pulled, how that angle was maintained, strip direction, test rate, temperature and any reinforcement applied to the arm. A study by Oreski and Pinter compared arrangements for peeling layers of two PV backsheets. The authors found that peel-arm deformation and orientation affected the measured response of their specimens. They examined a reinforced arrangement for those backsheets. For a buyer, the practical implication is to record the actual arrangement used by each supplier. There is no basis in that study for requiring the same reinforcement for every module material.
The classic NREL study of EVA adhesion on glass also describes how stretching of the encapsulant and the choice of backing complicated interpretation. If a supplier changes backing film to keep specimens from breaking, retain a method revision and a specimen diagram with the new results. Use a common reference construction in both methods if engineering needs to relate old and new results. If the evidence cannot support that relationship, start a separate series.
In a reliability review, combine adhesion evidence with the other observations that triggered the question. A picture of separation after a damp-heat sequence is worth documenting, as is a mechanical test on sister specimens taken through the same sequence. Neither observation is a clock for predicting field life in years. Use the guide to PV module thermal cycling and damp heat to keep the full module exposure record associated with the material evidence. A procurement decision about acceptance after conditioning should say which property and configuration it covers.
Review two offers without mixing their claims
Consider this hypothetical bid review. A distributor is buying a replacement run of panels after an approved backsheet becomes unavailable. The electrical design stays the same. Offer A includes a current film maker's backsheet peel row and a specimen photograph with no sample ID. Offer B includes a coupon report that identifies the proposed rear encapsulant and new sheet, with photographs showing that an inside layer of the backsheet tore. Neither offer supplies a direct numerical result for the requested rear interface in the proposed construction.
For offer A, ask which backsheet was used to generate the published material figure and how it relates to the candidate part. A revised technical datasheet can be a legitimate answer to a materials screening question. To close the change approval, require the module supplier to connect the candidate backsheet and encapsulant to a representative sample and the proposed production process. A fresh photograph alone would still leave the link between sample and drawing unresolved.
For offer B, record that the material pairing and specimen identity have been supported. Keep the reported failure inside the backsheet as a finding in its own right. Ask the test engineer whether a valid target-interface result was obtained anywhere on the trace, whether another method can isolate the interface, and what design decision the internal tear affects. Do not assign an unmeasured interface the value reached just before the tear. If the project's documented criterion allows an alternative failure outcome, obtain its signed interpretation for this exact setup.
Those responses can change a sourcing decision even before numerical results arrive. You might authorize a limited sample build using B's documented pairing and hold the volume release pending identification of the failure path. You might continue considering A for a different build whose only requirement at the current stage is film selection. Neither outcome requires calling one product inferior. Each follows from the decision the documents can actually support.
If you already have two reports with different units or failure locations, send the module drawing, target interface and redacted report headings with your RFQ. Identify the decision date and whether a sample build can proceed while the evidence is reviewed. Those details let a supplier quote the evidence work separately from the modules and state exactly what the first delivery will include.
Agree how the laboratory will report exceptions
A useful report keeps every planned specimen visible, including a strip that slipped at the grips or broke before reaching stable separation. Ask the lab for a disposition next to each specimen ID. Where a value is excluded from a calculated mean, request the technical reason and the rule used. This protects both sides: a visible equipment problem need not be silently counted as a weak bond, and an inconvenient material failure cannot quietly disappear from the average.
For the valid traces, ask for individual values with their matching failure descriptions and a summary suitable for the agreed acceptance rule. If the rule applies to individual specimens, an attractive mean cannot establish compliance on its own. If it applies to a group statistic, do not retroactively substitute a minimum after seeing the results. Confirm in writing who can approve a retest, what specimens it will cover, and how superseded results stay linked to the initial report.
Separate a missing detail from an adverse finding. If the material lot is legible in a production record and missing only on the report cover, a corrected traceability page may resolve the problem. If the reported sample was made from last year's backsheet, correcting the cover would misrepresent it. Keep the result as historical evidence and ask for a documented equivalence argument or a sample of the actual new construction. This distinction can save a second test when the issue is clerical without treating a different laminate as proven.
A test lab may be able to share photographs and reduced traces more readily than proprietary process settings. Agree on the minimum data to be released to the buyer and on any records available for controlled review. For a simple repeat purchase, a report reference and proof that the approved materials and process remain applicable may be enough under the purchase agreement. For an unresolved material substitution, obtain the full change disposition before treating the repeat order as routine.
Put the release conditions in the purchase order
Give the order a short evidence schedule with an owner and a deadline for each deliverable. For example, have purchasing supply the module revision and quantity, the manufacturer identify the mating materials and specimen design, and the responsible engineer approve the test conditions and decision rule. Have the party that runs the test supply the trace, the two separated faces and its interpretation. Agree who has final authority to release the modules if the specimen separates at a different interface.
Make the order clear about what can move while a question remains open. It may permit preparation of a pilot lot, authorize shipment of identified samples, or require a hold on all affected volume units. Write down the affected part numbers and end condition for the hold. A purchasing employee who was absent from the technical discussion should be able to tell whether a revised report or a fresh evaluation is required before authorizing shipment.
When the issue comes from a field return, preserve the panel identity, installation context and photographs before agreeing to destructive examination by a qualified party. Mark the area of concern on a diagram and agree whether an apparently unaffected region is available as a comparison. Trace any associated production lots through the supplier. Separate the finding on the returned product from the decision about new stock. A damaged return and a newly made witness sample can inform the same investigation without representing the same population.
Leave the target value blank until the design owner identifies the applicable written criterion and approves its meaning for that construction. Then enter the method revision, statistic, units, exposure state and allowable failure classifications next to it. Procurement can check completeness of that record. Authority for setting an engineering limit and accepting departures should remain with the people responsible for the design and its use.
Buyer FAQ
Is a backsheet peel value enough for a glass-glass module?
First check the specimen drawing. A result for a bond to a polymer backsheet addresses a material that may be absent from your construction. Ask for the front or rear glass surface specified by your drawing, the mating encapsulant, and representative process conditions. If the supplier relies on evidence from a different stack, require its written scope and the design owner's acceptance before using it to release the model.
Can cure data replace the peel report?
A cure measurement answers a different materials question. It can help identify process differences when interpreting a weak bond, but it does not show where a finished laminate separates under the agreed test. Keep the cure measurement and the interface result under their own identifiers. The PV encapsulant cure evidence guide explains how to specify the corresponding cure evidence.
Does a torn film mean the target bond passed?
It shows that this specimen tore under the recorded conditions. The target bond may have remained intact during that event. To classify the outcome as a pass, check the written criterion for this construction and ask the reviewing engineer to apply it. If the order specifically requires a measured target-interface value, document that this test did not return one.
Can one supplier quote an energy value and another quote peel strength?
They can report their own methods, but a ranking needs a common decision rule. Confirm that the energy result identifies the method and interface, and that the peel result identifies force per width and geometry. If one offer requires a new test for a comparable decision, price and schedule that work explicitly. Retain the original results for the separate questions they can answer.
How should we price destructive samples for a small order?
Ask each bidder to separate the module quantity for sale, the cost of any dedicated coupons or modules, the laboratory charge, and any independent witnessing or shipping. Ask which technical question each expense resolves. If an existing authenticated report applies to an unchanged approved construction, your engineer can assess its suitability before paying for duplicate tests. Obtain the dates and delivery implications from the party doing the work.
What if the supplier cannot identify the backsheet formulation?
Ask for a controlled grade code, revision and surface designation, with a supplier statement linking them to the specimen and the quoted production materials. Agree how future changes will be notified. If the code is reused for several untracked compositions, the report cannot establish which one is proposed. An independent confidential review may resolve a legitimate disclosure limit if both parties agree on the information it will confirm.
What should receiving personnel do with a delivery under conditional release?
Match the delivery's part number, revision and lot to the signed disposition, then check the permitted action. An approval to receive sample units does not authorize their use in the finished project. If the lot is outside the approved scope, segregate the affected stock according to your receiving procedure and contact the release owner. Keep the relevant report and release instruction accessible to the people making the physical stock decision.
Request evidence for the module you intend to buy
For a custom assembly, start with the project description on the SINAWATTS OEM procurement page. Include the proposed module revision, the two materials at the bond of interest, the decision you need to make, and any existing evidence you have permission to share. Request a quote that identifies the sample, the report deliverables and the approval needed before shipment. Ask the respondent to distinguish existing documents from work that requires a separate quotation so both parties can plan the release against the same evidence.